FugaPower® Regular CG1

  • About Product

FugaPower Regular CG1 - A cement-based, colored joint filler material used for indoor applications.


Conforms to EN 13888 – CG1 class:

  • CG = cement-based joint filler
  • 1 = normal joint filler material


Application Areas

  • Used indoors, in vertical and horizontal applications, for filling joints between tiles, ceramics, granite, marble, and mosaics
  • Applied in buildings, shopping centers, hotels, kitchens, bathrooms, and hallways


Advantages

  • Contains silicone
  • Maintains its color for a long time
  • Easy to prepare and apply
  • Does not scratch sensitive surfaces
  • Suitable for joint widths of 1-6 mm
  • Adheres to the edges of ceramics without cracking
  • Long working time
  • Reduced water absorption
  • Available in a wide range of colors

Product order

Click to order the product faster

Make Order

FugaPower Regular CG1 - A cement-based, colored joint filler material used for indoor applications.


Conforms to EN 13888 – CG1 class:

  • CG = cement-based joint filler
  • 1 = normal joint filler material


Application Areas

  • Used indoors, in vertical and horizontal applications, for filling joints between tiles, ceramics, granite, marble, and mosaics
  • Applied in buildings, shopping centers, hotels, kitchens, bathrooms, and hallways


Advantages

  • Contains silicone
  • Maintains its color for a long time
  • Easy to prepare and apply
  • Does not scratch sensitive surfaces
  • Suitable for joint widths of 1-6 mm
  • Adheres to the edges of ceramics without cracking
  • Long working time
  • Reduced water absorption
  • Available in a wide range of colors


Technical Indicators

  • Composition: Special cement, mineral fillers, polymer
  • Compressive strength - EN 12808: 3 ≥ 15 N/mm²
  • Flexural strength - EN 12808: 3 ≥ 2.50 N/mm²
  • Water absorption - EN 12808: 5 - 30 min ≤ 5 g, 240 min ≤ 10 g
  • Abrasion resistance - EN 12808: 2 ≤ 2000 mm³
  • Shrinkage - EN 12808: 4 ≤ 3 mm/m
  • Surface temperature for application: +5°C - +25°C
  • Service temperature: -20°C - +80°C
  • Mixture density: ~ 1.90 kg/L
  • Consumption varies based on tile size and joint width. The above indicators were measured at +23°C and 50% relative humidity. Higher temperatures shorten the time, while lower temperatures extend it.
CompositionSpecial cement, mineral fillers, polymer
Compressive strength3 ≥ 15 N/mm²
Flexural strength3 ≥ 2.50 N/mm²
Water absorption5 - 30 min ≤ 5 g, 240 min ≤ 10 g
Abrasion resistance2 ≤ 2000 mm³
Shrinkage4 ≤ 3 mm/m
Surface temperature for application+5°C - +25°C
Service temperature-20°C - +80°C
Mixture density~ 1.90 kg/L